Specially used in preselecting and removing gangue when discharging coarse particles(0-18mm).
Magnetic field intensity: 250-450 mT.
Feeding iron grade is improved by greatly removing gangue.
Greatly improving handling capacity, reducing milling cost, remarkable economic advantage.
Parameter of wet medium-intensity premilling gangue-removing magnetic separator
Model |
Drum dimensions
mm |
Average magnetic intensity of drum surface at ore seprating
mT |
Rotation speed of the drum
r.p.m |
Separating particle size
mm |
Capacity
t/h |
Motor model |
Motor power
kw |
W
kg |
CT2-66 |
φ600×600 |
250-450 |
42 |
0-16 |
8-15 |
XWD1.5-4-35 |
1.5 |
825 |
CT2-69 |
φ600×900 |
12-20 |
XWD2.2-4-35 |
2.2 |
999 |
CT2-79 |
φ750×900 |
35 |
0-18 |
15-30 |
XWD3-4-43 |
3
3 |
1375 |
CT2-712 |
φ750×1200 |
20-40 |
1834 |
CT2-99 |
φ900×900 |
31 |
25-50 |
XWD-4-4-47 |
4
4 |
1540 |
CT2-912 |
φ900×1200 |
30-60 |
2053 |
CT2-916 |
φ900×1600 |
35-75 |
XWD5.5-4-47 |
5.5 |
2637 |
CT2-1010 |
φ1050×1000 |
21 |
40-80 |
XWD7.5-4-71 |
2700 |
CT2-1015 |
φ1050×1500 |
50-100 |
7.5 |
3300 |
CT2-1020 |
φ1050×2000 |
60-120 |
5400 |
CT2-1212 |
φ1200×1200 |
17 |
80-150 |
XWD7.5-4-87 |
5325 |
CT2-1218 |
φ1200×1800 |
100-180 |
5700 |
CT2-1224 |
φ1200×2400 |
150-220 |
XWD11-4-87 |
11 |
6500 |